The flotation tests found that the flotation recovery of fine hematite increased observably to 94.51% from 68.69% by adding 4 mg/L PAAS before NaOL at pulp pH 7.3; in the separation of mixed hematite and quartz, the separation efficiencies of fine hematite with and …